AbstractEvaporation of Pb and Li from molten Pb17Li was investigated between 350 and 800°C in vacuum, argon and helium covergas. Results were also obtained from other experimental facilities. Similarities were found to observations from sodium cooled reactors.The results show that Pb and Li evaporate independent on each other. The two elements show different behavior along the transport pathway. Deposits of the evaporated metals contained between 0.2 and 98 at% Li. As in the reactor RAPSODIE for sodium, evaporation rates for lithium were smaller in helium than in argon, however evaporation rates of lead were the same in both gases. No aerosol problems will exists with normal blanket operation. Under experimental conditions, aerosol concentrations were in the range of 10−9 to 10−6 g/m3. Aerosols can easily be trapped with sintered metal filters.
溶融Pb-17LiからのPbとLiの蒸発を、真空中およびアルゴン・ヘリウムカバーガス中で350〜800°Cの温度範囲において調査した。他の実験施設でも同様の結果が得られた。ナトリウム冷却原子炉での観察結果との類似性が見出された。結果は、PbとLiが互いに独立して蒸発することを示している。この2つの元素は輸送経路に沿って異なる挙動を示す。蒸発した金属の堆積物には、0.2〜98at%のLiが含まれていた。ナトリウムに関するRAPSODIE原子炉の場合と同様に、リチウムの蒸発速度はヘリウム中よりもアルゴン中で小さかったが、鉛の蒸発速度は両ガス中で同じであった。通常のブランケット運転では、エアロゾルによる問題は発生しない。実験条件下では、エアロゾル濃度は10⁻⁹〜10⁻⁶g/m³の範囲であった。エアロゾルは焼結金属フィルターで容易に捕集できる。